As the professional manufacturers, Top Bearings would like to provide you high quality CuZn31Si Silicon Brass Wrapped Bronze Bearing Antifatigue. And we will offer you the best after-sale service and timely delivery.
As the professional manufacturers, Top Bearings would like to provide you high quality CuZn31Si Silicon Brass Wrapped Bronze Bearing Antifatigue. And we will offer you the best after-sale service and timely delivery.
Material: |
CuZn 31 Si Bronze Bushings |
Types: |
ASB Z90 F Rolled (wrapped) Bronze Bushings With Diamond Indents |
Application: |
Agricultural, Building And Engineering Machines, Etc. |
Supply Ability: |
Perforated Bronze Bearing,Plain Bronze Wrapped Bearings |
High Light: |
CuZn31Si Wrapped Bronze Bearing, Antifatigue Wrapped Bronze Bearing, ISO16949 Wrapped Bronze Bearing |
091 bronze wrapped bushing with groove 40*36*82 metric size
40*36*82mm, the Chemical formula of the alloy is CuZn31Si. Silicon brass is characterized by high strength and corrosion resistance.
ISO 426-1 Grade CuZn31Si
Brass Wrapped Bushing, with material CuZn31Si. It has good anti-fatigue, anti-erosion and anti-abrasion and load capacity. It can be produced by different bronze material and the surface can be produced with other type of oil socket and oil groove in different working condition. The material structure, application fields, and technical parameter are as follows.
The use of parameters | |||||
Parameters | 090 Bronze Wrapped Bushing | 091 Copper Wrapped BushingBronze Wrapped Bushing | 092 Bronze Wrapped Bushing | 094 Bronze Wrapped Bushing | 09G Bronze Wrapped Bushing |
Density | |||||
8.9g/cm³ | 8.9g/cm³ | 8.4g/cm³ | 8.9g/cm³ | 8.9g/cm³ | 8.3g/cm³ |
Pressure resistance strength | 470N/mm² | 440N/mm² | 470N/mm² | 470N/mm² | 470N/mm² |
Coefficient of heat | 60W/m.k | 71W/m.k | 60W/m.k | 60W/m.k | 58W/m.k |
Linear expansion coefficient | 18.5×10-6/K | 19.2×10-6/K | 18.5×10-6/K | 18.5×10-6/K | 18.5×10-6/K |
Hardness | 90~120 HB | 80~110 HB | 90~120 HB | 90~120 HB | 90~120 HB |
Elongation | 55% | 30% | 55% | 55% | 55% |
Alloy material | CuSn8P | CuZn31Si | CuSn8P | CuSn8P | CuSn8P |
Other material | CuSn6.5P | CuSn6.5P | CuSn6.5P | CuSn6.5P |
working temperature
|
-40~+150℃
|
|
Coefficient of linear expansion
|
19.2×10-6/K
|
|
Friction coefficient
|
0.06~0.15μ
|
|
Mating Axis
|
Hardness
|
≥50
|
Roughness
|
0.4~1.0
|